2026-01-30•6 min defect fix•VIESUNCO Materials Science Team

Shopfloor Injection Fix: 4 Tuning Tricks to Stop TPE Flash & Surface Delamination

Manual trimming of flash eats your profits. Learn optimal cavity vent depth (0.015mm), V/P switchover points, and barrel shear management to eliminate flash and peeling.

#Mold Flash#Delamination#Cavity Venting#Injection Tuning#Defect Fix
Shopfloor Injection Fix: 4 Tuning Tricks to Stop TPE Flash & Surface Delamination

1. Why TPE Flashes Easily

TPE is a shear-thinning polymer with low melt viscosity under high pressure:

Technician Checking Part Parting Line at Injection Machine
▲ Technician Checking Part Parting Line at Injection Machine
  • Vent Depth: Venting slots must be machined between 0.012mm and 0.018mm.
  • V/P Switchover: Switch to holding pressure when cavity is 95%–98% filled.

Need a Custom TPE/TPR Formulation for Your Application?

Our polymer engineering team provides 1-on-1 technical consulting, tooling support, and complimentary testing samples.